What forensic physics examines
Forensic physics studies physical evidence: glass, paint, soil, fibres, tool marks, building materials and metals, and the forces involved in accidents. The goal is to identify materials, compare them with possible sources, and reconstruct events. Most of these materials are class evidence: they can show that two samples could share a source, but rarely that they must.
Glass
Glass turns up in burglaries, hit-and-runs, shootings and explosions. It is an amorphous (non-crystalline) solid made mostly of silica (SiO2) with other oxides added.
| Type | Main ingredients | Common uses |
|---|---|---|
| Soda-lime | SiO₂ + Na₂O + CaO | Windows, bottles |
| Borosilicate | SiO₂ + B₂O₃ | Laboratory glassware, some headlamps |
| Lead (flint) | SiO₂ + PbO | Lenses, fine glassware |
| Tempered (toughened) | Heat-treated soda-lime | Vehicle side windows; breaks into small cubes |
| Laminated | Two glass sheets with a plastic (PVB) layer | Windscreens; cracks but holds together |
Reading fractures
When something strikes a pane, two kinds of crack form:
- Radial cracks spread outward from the point of impact, like spokes. They form first, on the side opposite the blow.
- Concentric cracks form circles around the impact point, on the same side as the blow.
Two further rules help reconstruction:
- Sequence of impacts. A new crack stops when it reaches an existing one. So when there are two holes, the one whose cracks stop at the other's cracks was made second.
- Direction of force: the 3R rule. On the broken edge of a Radial crack, curved stress lines (rib marks) meet the Reverse side (away from the force) at a Right angle.
Interactive diagram
Reading broken glass
Fracture patterns can show where glass was struck, from which side, and in what order. Select each pattern.
Radial cracks spread out from the impact point
When an object strikes glass, the glass bends away from the blow. The side opposite the impact stretches most, so cracks start there and run outwards from the point of impact like the spokes of a wheel.
Radial cracks form first, on the side opposite the force.
Simplified drawings. Tempered and laminated glass break differently and need specialist interpretation.
Tap each pattern to see how it forms
Laboratory comparison
- Physical fit: if a fragment fits exactly into a broken edge, it is very strong evidence the two were once one piece.
- Refractive index (RI): how much glass bends light. Fragments are immersed in an oil whose RI changes with temperature; at the temperature where the fragment's edge (the Becke line) disappears, the oil and glass have the same RI. GRIM (glass refractive index measurement) automates this.
- Density: compared by flotation in liquids of known density.
- Colour and thickness: by microscopy and spectrophotometry.
- Elemental composition: by XRF, SEM-EDX, ICP-MS or LA-ICP-MS (laser ablation), and laser-induced breakdown spectroscopy (LIBS). Trace elements can separate glasses that look and measure the same.
Reports usually say the fragments are "indistinguishable from" or "consistent with" the known glass, or that they "could not have come from" it. A single source is rarely claimed, because many panes share the same properties.
Pause and answer
- Two bullet holes are close together in a window. The cracks from hole X stop at the cracks from hole Y. Which shot came first?
- Why is a matching refractive index not proof that glass came from one window?